Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 22 dynes/cm | 22 dynes/cm | 25°C |
LyondellBasell Ethanol, 200 Proof Information provided by Lyondell. |
|||
Surface Tension | 22 dynes/cm | 22 dynes/cm | 25°C |
LyondellBasell TBAcâ„¢ Solvent, Tertiary butyl acetate Information provided by Lyondell. |
|||
Surface Tension | 22 dynes/cm | 22 dynes/cm | ASTM D1331 |
Solvay Specialty Polymers FOMBLIN® Y L-VAC 14/6 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |
|||
Surface Tension | 22 dynes/cm | 22 dynes/cm | ASTM D1331 |
Solvay Specialty Polymers FOMBLIN® Y L-VAC 16/6 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |
|||
Surface Tension | 22 dynes/cm | 22 dynes/cm | ASTM D1331 |
Solvay Specialty Polymers FOMBLIN® Y L-VAC 25/6 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |
|||
Surface Tension | 22 dynes/cm | 22 dynes/cm | ASTM D1331 |
Solvay Specialty Polymers FOMBLIN® Y25 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |
|||
Surface Tension | 22 dynes/cm | 22 dynes/cm | ASTM D1331 |
Solvay Specialty Polymers FOMBLIN® Y45 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |