Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Surface Tension 20.1 dynes/cm
20.1 dynes/cm
Dow Corning XIAMETER® PMCPPMX-200 10CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 10CS. 100% active, 10 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning