Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 170 - 325 Mesh | 170 - 325 Mesh | |
Potters Industries Spheriglass® 2530 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Particle Mesh Size | 200 - 325 Mesh | 200 - 325 Mesh | 0.0188 |
Gromax Melamine (Fine Grade) China KInformation provided by Gromax Enterprises Corp. |
|||
Particle Mesh Size | 200 - 325 Mesh | 200 - 325 Mesh | 0.2153 |
Gromax Standard GB9567-97 China NInformation provided by Gromax Enterprises Corp. |
|||
Particle Mesh Size | 200 - 325 Mesh | 200 - 325 Mesh | 0.2285 |
Gromax Standard GB9567-97 China SInformation provided by Gromax Enterprises Corp. |