Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 16 - 20 Mesh | 16 - 20 Mesh | US Sieve |
Potters Industries A-Series A-100 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Mesh Size | 16 Mesh | 16 Mesh | Irregular shape. ETM = Equistar Test Method; ETM Malvern |
LyondellBasell Microthene® G MN72700 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Particle Mesh Size | 16 Mesh | 16 Mesh | 0.8% retained; U.S. Sieve |
Imerys Minsilsparâ„¢ 1 Feldspar Minsilspar 1 is a feldspathic sand (sandspar).Information provided by Imerys |
|||
Particle Mesh Size | 16 Mesh | 16 Mesh | Opening 1700µm; ASTM E11 |
Solvay Chemicals SOLID CAUSTIC SODA MICROPEARLS Some applications of this product may be regulated or restricted by national or international standards (e.g. for food additives, water treatment, the pharmaceutical industry, etc). The buyer and th.. |
|||
Particle Mesh Size | 16 Mesh | 16 Mesh | 1.9% passing, dry |
CIMBAR Suspengel™ 16 High Purity Bentonite, Industrial Grade Suspengel products are manufactured from the highest quality Western Bentonite reserves. Suspengel products are easy to disperse thixotropes with excellent suspension properties. Strict process co.. |