Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brookfield Viscosity = 960 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 760 - 960 cP

@Temperature 25.0 °C
760 - 960 cP

@Temperature 77.0 °F
C.O.I.M. EXTER S® S 101 Orthophthalic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 101: Medium/high rea..
Copyright © lookpolymers.com All Rights Reserved