Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 9000 cP @Temperature 25.0 °C |
9000 cP @Temperature 77.0 °F |
Toluene solution. Neat polymer concentration, 25%w. |
Kraton® D1116 (SB)n Branched Copolymer (SB)n - styrene-butadiene multi-arm (branched) copolymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve .. |
|||
Brookfield Viscosity | 9000 cP | 9000 cP | 20 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® 45 PVC PVC Copolymer Dispersion Resin F-45 is a vinyl chloride vinyl acetate copolymer dispersion resin with low paste viscosities, excellent heat stability, and rapid fusion characteristics. F-45 has been.. |
|||
Brookfield Viscosity | 9000 - 16000 cP | 9000 - 16000 cP | Zeon Test #170 |
Zeon Chemicals Nipol® 1312LV Liquid Nitrile Elastomer Nipol 1312LV is a copolymer of butadiene and acrylonitrile with medium oil resistance in liquid form. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Sa.. |
|||
Brookfield Viscosity | 9000 - 12000 cP | 9000 - 12000 cP | RVF/RVT #6 sp @ 80°F |
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives 3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M |
|||
Brookfield Viscosity | 9000 cP | 9000 cP | Thermosel using spindle #27 |
3M Scotch-Weld™ TE100 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Brookfield Viscosity | 9000 cP | 9000 cP | Thermosel using spindle #27 |
3M Scotch-Weld™ TS230 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Brookfield Viscosity | 9000 - 16000 cP | 9000 - 16000 cP | Accelerator, RVF #6 spindle, 20 rpm @ 27°C |
3M Scotch-Weld™ DP-100 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP-100 is a two-part adhesives offering fast cure and machinability.Information provided by 3M |
|||
Brookfield Viscosity | 9000 cP | 9000 cP | Thermosel using spindle #27 |
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |