Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 5000 - 9000 cP | 5000 - 9000 cP | DOP 60phr, 6RPM; ASTM D1824-90 |
LG Chemical LK170 PVC General Description: LK170, vinyl chloride copolymer with vinyl acetate exhibit excellent properties including easy processing and effective flowMain Applications: Sealant, automotive protective sol.. |
|||
Brookfield Viscosity | 5000 - 9000 cP | 5000 - 9000 cP | Accelerator, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |