Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 8250 cP @Temperature 121 °C |
8250 cP @Temperature 250 °F |
|
3M Scotch-Weld™ 3776LM Low Melt Adhesive Bonds variety of plastics, woods and light-gauge metals and use with low melt applicator onlyInformation provided by 3M |