Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 800 cP | 800 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 5570 Styrene - Butadiene Copolymer Europrene Latice® 5570 is an aqueous anionic dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does no.. |
|||
Brookfield Viscosity | 800 cP | 800 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 5577 Styrene - Butadiene Copolymer Europrene Latice® 5577 is an aqueous anionic dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does no.. |
|||
Brookfield Viscosity | 800 - 1200 cP @Temperature 20.0 °C |
800 - 1200 cP @Temperature 68.0 °F |
Brookfield RVF sp. 2, 20 rpm solution at 15% in MEK; MQSA N0 40A |
Lubrizol Advanced Materials Pearlstick® 45-50/08 Linear Thermoplastic Polyurethane Elastomer
(discontinued ** Pearlstick 45-50/08 is an elastic, linear, aromatic polyurethane with an extremely high crystallization rate and a medium-low thermoplasticity level, available as pellets.Solubility: Pearlstick 45-.. |
|||
Brookfield Viscosity | <= 800 cP | <= 800 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 5044 SBR Latex ROVENE® 5044 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of permanent label and construction adhesives. Its relative low molecular w.. |
|||
Brookfield Viscosity | <= 800 cP | <= 800 cP | #20/200 |
Mallard Creek Polymers Rovene® 6021 Styrene-Acrylic Emulsion Applications: Rovene® 6021 is a soft, carboxylated styrene-acrylic copolymer emulsion. The typical films are soft and strong with good water resistance and exhibit good resistance to discoloratio.. |
|||
Brookfield Viscosity | <= 800 cP | <= 800 cP | #20/200 |
Mallard Creek Polymers Rovene® 6025 Styrene-Acrylic Emulsion Applications: Rovene® 6025 can be used in multiple coating and paint applications including landscaping coatings and low sheen interior flat wall coatings. It can also be used as a binder for dus.. |
|||
Brookfield Viscosity | 800 cP @Temperature 25.0 °C |
800 cP @Temperature 77.0 °F |
20 RPM |
KaMin Hydramatte® Kaolin Clay - Filler Hydramatte® is a coarse delaminated clay designed for low gloss applications such as matte and dull finishes.Industry: PAPER & PACKAGINGUses: Coated Freesheet/Art Paper, Coated 1S Label, Coated .. |
|||
Brookfield Viscosity | 800 cP @Temperature 25.0 °C |
800 cP @Temperature 77.0 °F |
20 RPM |
KaMin Polyplate® HMT Kaolin Clay - Delaminated Polyplate® HMT is a high brightness, very high aspect ratio, delaminated kaolin, intended for use in water-borne coatings, adhesives, and sealants. The large, platy structure of Polyplate® HMT.. |
|||
Brookfield Viscosity | <= 800 cP | <= 800 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4423 SBR Latex ROVENE® 4423 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of permanent label adhesives. Its relative high molecular weight and styren.. |
|||
Brookfield Viscosity | 800 cP @Temperature 125 °C |
800 cP @Temperature 257 °F |
|
Westlake Epolene® E-10 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Epolene® E-Type Polymers are easily emulsifiable, available in PE and PP based materials, and approved by the FDA for food contact. They have a wide ring & ball softening point range, oil and water.. |
|||
Brookfield Viscosity | <= 800 cP | <= 800 cP | #2 @ 50 rpm |
Dow Latex LXC 771NA Carboxylated Styrene-Butadiene Latex Applications: Dow Latex LXC 771NA is a high solids, high performance latex that offers many benefits over standard styrene-butadiene latexes in carpet applications. Dow Latex LXC 771NA is a unique p.. |
|||
Brookfield Viscosity | 800 - 1600 cP | 800 - 1600 cP | RVT #3 sp @ 20 rpm |
3M Scotch-Weld™ TL22 Threadlocker Anaerobic Adhesive 3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening.. |
|||
Brookfield Viscosity | 800 - 1600 cP | 800 - 1600 cP | RVT #2 sp @ 20 rpm |
3M Scotch-Weld™ TL42 Threadlocker Anaerobic Adhesive 3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening.. |
|||
Brookfield Viscosity | 800 - 1600 cP | 800 - 1600 cP | RVT #2 sp @ 20 rpm |
3M Scotch-Weld™ TL62 Threadlocker Anaerobic Adhesive 3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening.. |
|||
Brookfield Viscosity | 800 - 1300 cP | 800 - 1300 cP | RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in THF |
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane Features: It has the highest heat resistance of any Estane TPU resin used in adhesives. Supplied as pale amber granules, it is soluble in THF or THF/MEK blends. Higher heat resistance, tensile and b.. |