Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 80 - 200 cP | 80 - 200 cP | LVT, Spindle #3 @ 30rpm |
Lord Adhesives Flocklok® 853A Flock Adhesive LORD Flocklok® 853A is a blocked, heat-curing, singlecoat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates pro.. |
|||
Brookfield Viscosity | 80 cP @Temperature 200 °C |
80 cP @Temperature 392 °F |
Melt |
Zeon Chemicals Quintone® U190 Aliphatic Hydrocarbon Resin C5/C9 type (piperylene and dicyclopentadiene precursor).Information provided by Zeon Chemicals L.P. |
|||
Brookfield Viscosity | 80 - 120 cP @Temperature 25.0 °C |
80 - 120 cP @Temperature 77.0 °F |
Brookfield LVF, Spindle 1-60 RPM |
BCC Products BC 100 Medium Cyanoacrylate Adhesive BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas.. |
|||
Brookfield Viscosity | 80 - 120 cP | 80 - 120 cP | |
3M Scotch-Weld™ EC100 General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |