Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 3700 cP | 3700 cP | RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in Cyclohexanone |
Lubrizol ESTANE® 5714 Ether Based Thermoplastic Polyurethane Features: Low Temperature Flexibility, Excellent Abrasion, Fungal, and Chemical Resistance, and Hydrolytic Stability. Adhesives can be applied from solution or extruded as a melt coating. The resin .. |