Polymer Property : Brookfield Viscosity = 3250 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity >= 3250 cP
>= 3250 cP
0.3% in 1% HCl, LV3 rpm spindle n°2 after 24 h at 40°C; TI-2102-1
Solvay RHEOZAN Biopolymer
Description: Biopolymer: very stable in acid media (such as sulfuric acid). Highly pseudoplastic.Identification: SUCCINOGLYCAN GUMCAS: 73667 – 50 – 2Available in: Asia Pacific, Europe, Lat..
Brookfield Viscosity 3250 cP

@Temperature 23.9 °C
3250 cP

@Temperature 75.0 °F
#2 spindle @ 20 rpm
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting
BC8010-2 Metal-Kast/Slo, the result of extensive research and development is an aluminum filled, metal-like, medium setting urethane reproduction plastic. A slower version of the BC8010 Metal-Kast w..
Brookfield Viscosity 3250 cP
3250 cP
melt viscosity
Kuraray SEPTON® A1 Hot Melt Adhesive
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. Using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic block c..