Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 30000 cP | 30000 cP | 20 rpm; ISO 2555/4575 |
SABIC PVC 701E Emulsion Polyvinyl Chloride for Paste Preparation Product Description: PVC 701E is a fine particle, medium-molecular weight PVC homopolymer, made by emulsion polymerization. It is designed for the manufacture of plastisols exhibiting high viscosi.. |
|||
Brookfield Viscosity | 30000 cP @Temperature 23.9 °C |
30000 cP @Temperature 75.0 °F |
|
3M Scotch-Weld™ 3532 B/A Brown Two-Part Urethane Adhesive 3532 B/A Brown
(discontinued **) Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 20-30 minutes handling stren.. |
|||
Brookfield Viscosity | 30000 cP @Temperature 23.9 °C |
30000 cP @Temperature 75.0 °F |
|
3M Scotch-Weld™ 3535 B/A Off-white Two-Part Urethane Adhesive 3535 B/A Off-white
(discontinued **) Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 15-20 minutes handling stren.. |
|||
Brookfield Viscosity | 30000 cP @Temperature 23.9 °C |
30000 cP @Temperature 75.0 °F |
|
3M Scotch-Weld™ 3549 B/A Brown Two-Part Urethane Adhesive 3549 B/A Brown
(discontinued **) Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include long worklife adhesive, 2-4 hours handling stren.. |
|||
Brookfield Viscosity | 30000 cP | 30000 cP | 20 rpm; ISO 2555/4575 |
SABIC PVC 741E Emulsion Polyvinyl Chloride for Paste Preparation Product Description: PVC 741E is a fine particle, high molecular weight PVC homopolymer, made by emulsion polymerization. It is designed for the manufacture of plastisols exhibiting low viscositie.. |
|||
Brookfield Viscosity | 30000 - 50000 cP @Temperature 25.0 °C |
30000 - 50000 cP @Temperature 77.0 °F |
HBT, Spindle #SC4-14 @ 10rpm |
Lord Adhesives Metech 2539A Silver-Silver Chloride Reference Electrode Ink Silver-silver chloride reference ink is designed for screen print application onto flexible and rigid plastic substrates. It has been developed to provide a standard reference electrode potential ut.. |
|||
Brookfield Viscosity | 30000 - 44400 cP @Temperature 25.0 °C |
30000 - 44400 cP @Temperature 77.0 °F |
Spindle 6 @ 10rpm |
Lord Adhesives Circalokâ„¢ EP-939 Epoxy Board Level Encapsulant LORD Thermosetâ„¢ EP-939 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by.. |
|||
Brookfield Viscosity | 30000 cP | 30000 cP | 25% toluene solution; MA 04-3-064 |
Dynasol Solprene® 416 Thermoplastic Rubber SBS Dry Solprene 416 is a radial styrene/butadiene block copolymer having 30% of styrene content, most of it forming a polystyrenes block which gives the polymer a thermoplastic behavior. It develops proper.. |