Polymer Property : Brookfield Viscosity = 2.3 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 2.3 cP
2.3 cP
Initial Viscosity @ 2 rpmGeon® ATLC 22 (with provided formulation); Internal Method
PolyOne Geon™ FIT E 51 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® FIT E 51 is a medium molecular weight homopolymer resin intended for use as a Formulation Improvement Tool (FIT) in plastisol formulations which enhance the plastisol usage (pot life) and red..
Brookfield Viscosity 2.3 cP
2.3 cP
One Day Viscosity @ 2rpmGeon® ALTC 22 (with provided formulation); Internal Method
PolyOne Geon™ 210 Series 217 Blending Resin Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 217 is a low to medium molecular weight homopolymer blending resin intended for use as a formulation tool in plastisol formulations.It improves air release performance resulting in reduced sc..
Brookfield Viscosity 2.3 cP
2.3 cP
Initial Viscosity @ 2rpmGeon® ALTC 22 (with provided formulation); Internal Method
PolyOne Geon™ 210 Series 217 Blending Resin Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 217 is a low to medium molecular weight homopolymer blending resin intended for use as a formulation tool in plastisol formulations.It improves air release performance resulting in reduced sc..