Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 525 - 1850 cP | 525 - 1850 cP | RVT Spindle 3 @ 20 rpm |
Palm Labs Adhesives TURBO SEAL SERIES 55 BROWN FINE THREADS THREAD SEALANT TURBO SEAL SERIES 55 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures quickly in the absence of air between.. |