Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 180 - 450 cP @Temperature 23.0 °C |
180 - 450 cP @Temperature 73.4 °F |
|
Lucite International Series 100 Liquid Acrylic Resin LUCITE® LIQUID ACRYLIC RESINS SERIES 100For the manufacture of solid surface shapesAmbient temperature cureCan be used on batch or continuous in-line mixing equipmentInformation provided by Lucit.. |
|||
Brookfield Viscosity | 180 cP @Temperature 200 °C |
180 cP @Temperature 392 °F |
Melt |
Zeon Chemicals Quintone® D200 Aliphatic Hydrocarbon Resin C5/C9 type (piperylene and dicyclopentadiene precursor).Information provided by Zeon Chemicals L.P. |
|||
Brookfield Viscosity | 180 cP | 180 cP | #2 @ 50 rpm |
Dow Latex LXC 8429NA Carboxylated Styrene-Butadiene Latex Applications: Latex LXC 8429NA for carpet is a soft hand latex and is used in applications where a soft carpet hand is desired. These applications include some commercial and residential carpets, ru.. |
|||
Brookfield Viscosity | 180 - 200 cP | 180 - 200 cP | RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in Cyclohexanone |
Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane Features: It is especially well suited for dispersing co-ferrite as well as Cr02 pigments used in video, audio, and data storage applications. This product offers excellent hydrolytic stability unde.. |