Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 160000 - 220000 cP @Temperature 25.0 °C |
160000 - 220000 cP @Temperature 77.0 °F |
HBT, Spindle #SC4-14 @ 10rpm |
Lord Adhesives Metech 1130C Platinum Silver Conductor Composition This low cost, platinum silver conductor is designed for general hybrid applications. It employs advanced powders technology with a mix bonded frit system to yield a highly dense film that is resist.. |
|||
Brookfield Viscosity | 160000 cP | 160000 cP | 2 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® 25 PVC PVC Homopolymer Dispersion Resin F- 25 is a medium molecular weight PVC homopolymer dispersion resin with low residual surfactant content. Applications include caulk and sealants.Note 1. 500 gm resi.. |