Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 1400 - 1800 cP | 1400 - 1800 cP | Brookfield RVF sp 4, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 46-10/16 Polyester based TPU Pearlstick 46-10/16 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a high thermoplasticity level. Solubility: .. |
|||
Brookfield Viscosity | 1400 - 1800 cP | 1400 - 1800 cP | Brookfield RVF sp 4, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 45-80/16 Polycaprolactone based TPU Pearlstick 45-80/16 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a small amount of anti-adherent in the formulation. It has a very low crystalliz.. |
|||
Brookfield Viscosity | 1400 - 1700 cP | 1400 - 1700 cP | 1% KCl, LVT, 60 rpm, spindle 3; TI-1110 |
Solvay RHODICARE CFT Surfactant Description: Rhodicare® CFT is Cellulase-free clear grade of Xanthan Gum, it is recommended when associated with cellulose-based polymers. Approved for Ecocert. It is excellent anionic bio-polyme.. |
|||
Brookfield Viscosity | 1400 - 1700 cP | 1400 - 1700 cP | 1% in 1% KCl, LVT, 60 rpm, spindle 3; TI-1110 |
Solvay RHODICARE T Surfactant Description: Rhodicare® T is high purity grade specifically designed for thickening and suspension in clear formulations. It has high electrolyte stability over a wide range of pH and fast hydrat.. |
|||
Brookfield Viscosity | 1400 cP @Temperature -18.0 °C |
1400 cP @Temperature -0.400 °F |
|
ChevronTexaco Havoline® Type F Automatic Transmission Fluid Havoline Automatic Transmission Fluid Type F delivers value through:Protection against the formation of lacquers, sludge, or other harmful deposits.Exceptional stability provided by excellent base o.. |
|||
Brookfield Viscosity | 1400 - 1800 cP @Temperature 25.0 °C |
1400 - 1800 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 201 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 201: Polyester resin.. |
|||
Brookfield Viscosity | 1400 - 1500 cP @Temperature 23.9 °C |
1400 - 1500 cP @Temperature 75.0 °F |
Mixed, 1.5min |
BCC Products BC 8160 Urethane Casting BC8160 is a low viscosity two-component urethane casting compound that is specifically formulated for its flexural and impact strength. It is recommended for use for the production casting of highly.. |
|||
Brookfield Viscosity | 1400 - 1500 cP @Temperature 23.9 °C |
1400 - 1500 cP @Temperature 75.0 °F |
1.5 min mixed |
BCC Products BC 8860 Polyurethane Elastomer BC8860 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig.. |
|||
Brookfield Viscosity | 1400 - 3300 cP | 1400 - 3300 cP | 0.2% in water, 3 rpm; TI-2096 |
Solvay RHEOZAN SH Biopolymer Description: Biopolymer: very stable in acid media (such as sulfuric acid). Highly pseudoplastic.C.T.F.A. /I.N.C.I. Name: Succinoglycan GumCAS: 73667-50-2Soluble in waterCompatible with non-ionic, a.. |
|||
Brookfield Viscosity | 1400 cP @Temperature -18.0 °C |
1400 cP @Temperature -0.400 °F |
|
ChevronTexaco Type F Automatic Transmission Fluid General DescriptionType F is specifically designed for all pre-1977 Ford vehicles and some makes between 1977 and 1981. Effective March 1997, Ford discontinued administration of approvals for Type F.. |