Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 13500 cP | 13500 cP | 2 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® 45 PVC PVC Copolymer Dispersion Resin F-45 is a vinyl chloride vinyl acetate copolymer dispersion resin with low paste viscosities, excellent heat stability, and rapid fusion characteristics. F-45 has been.. |
|||
Brookfield Viscosity | 13500 cP @Temperature 23.9 °C |
13500 cP @Temperature 75.0 °F |
Mixed |
BCC Products BC 7136-2 Epoxy Casting BC7136-2 is an aluminum filled thick section casting system with heat resistance to 300ºF. May be cast to a thickness of 2 inches in non-conductive molds, 3 inches in conductive molds and thicker s.. |