Polymer Property : Brookfield Viscosity = 1.20e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 900000 - 1.20e+6 cP
900000 - 1.20e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-350 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are..
Brookfield Viscosity 900000 - 1.20e+6 cP
900000 - 1.20e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-350 Class B-12 Aerospace Sealant
3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are..
Brookfield Viscosity 900000 - 1.20e+6 cP
900000 - 1.20e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-350 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are..
Brookfield Viscosity 900000 - 1.20e+6 cP
900000 - 1.20e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-350 Class B-6 Aerospace Sealant
3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are..
Brookfield Viscosity 800000 - 1.20e+6 cP
800000 - 1.20e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-645 B-2 Aerospace Sealant
3M Aerospace Sealant AC-645 B-2 is a low density, two-component, manganese dioxide cured, liquid polysulfide polymer system. It is suitable for use in fuel tanks, fuselage hole filling, cavity filli..
Brookfield Viscosity 900000 - 1.20e+6 cP
900000 - 1.20e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-350 Class B-4 Aerospace Sealant
3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are..
Brookfield Viscosity 900000 - 1.20e+6 cP
900000 - 1.20e+6 cP
Base, RVF #7 sp @ 2 rpm
3M AC-350 Class B-1/4 Aerospace Sealant
3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are..