Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 20.0 cc/m²/day @Temperature 23.0 °C |
1.29 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Bicor™ 21MB777 OPP Film Product Description: Bicor 21MB777 is a high gas barrier, biaxially oriented transparent PP film coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging m.. |
|||
Oxygen Transmission Rate | 20.0 cc/m²/day @Temperature 23.0 °C |
1.29 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Bicor™ 26MB768 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VLTS) coating. PVdC provides an excellent moi.. |
|||
Oxygen Transmission Rate | 20.0 cc/m²/day @Temperature 23.0 °C |
1.29 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Bicor™ 26MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side acrylic. This film provides outstanding performance on all packaging mac.. |
|||
Oxygen Transmission Rate | 20.0 cc/m²/day @Temperature 23.0 °C |
1.29 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Bicor™ 32MB768 OPP Film Product Description: A High gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VTLS) coating. PVdC provides excellent moistu.. |
|||
Oxygen Transmission Rate | 20.0 cc/m²/day @Temperature 23.0 °C |
1.29 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Bicor™ 32MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging machin.. |
|||
Oxygen Transmission Rate | 20.0 cc/m²/day @Temperature 23.0 °C |
1.29 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Bicor™ 42MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent PP film, coated one side PVdC, one side acrylic, This film provides outstanding performance on all packaging machines.Availabi.. |
|||
Oxygen Transmission Rate | 20.0 cc/m²/day @Temperature 23.0 °C |
1.29 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 36MO747 OPP Film Product Description: A white opaque biaxially oriented polypropylene film acrylic coated on one side, one side PVdC. Provides outstanding performances on all packaging machines.Availability: Africa .. |
|||
Oxygen Transmission Rate | 20.0 cc/m²/day @Temperature 23.0 °C |
1.29 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 42AH748 OPP Film Product Description: A high barrier, high speed, super white opaque, modified higher density biaxially oriented polypropylene film, coated one side high barrier PVdC, one side very low temperature s.. |
|||
Oxygen Transmission Rate | 20.0 cc/m²/day @Temperature 23.0 °C |
1.29 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 50MO747 OPP Film Product Description: A white opaque biaxially oriented polypropylene film, coated on one side acrylic, one side PVdC. Provides excellent performance on all packaging machines.Availability: Africa & .. |
|||
Oxygen Transmission Rate | 20.0 cc/m²/day @Temperature 23.0 °C |
1.29 cc/100 in²/day @Temperature 73.4 °F |
Wet, 75% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 30MW747 OPP Film Product Description: White opaque biaxially oriented polypropylene film coated on one side acrylic, one side PVdC. Provides excellent performances on all packaging machines. 30MW747 is a super white.. |