Polymer Property : Oxygen Transmission = 70.0 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 1952 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2600 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
700 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2600 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2607 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2652 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
700 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2652 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2665 MAS071 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2665 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2667 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2800 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
700 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2800 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2805 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2805 MAS152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 3100 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
700 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 3100 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 3107 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
700 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® ET3117 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® ET2613 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® ET3127 Polycarbonate
Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® ET3227 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
178 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
2760 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® LQ2647 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g..