Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 65.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
165 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
650 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Oxygen Transmission | 65.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
165 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
650 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2607 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Oxygen Transmission | 65.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
165 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
650 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2805 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Oxygen Transmission | 65.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
165 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
650 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Oxygen Transmission | 65.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
165 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
650 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Oxygen Transmission | 65.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
165 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
650 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® ET3127 Polycarbonate Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist.. |
|||
Oxygen Transmission | 65.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
165 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
650 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® ET3227 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |