Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D3985 |
Eastman 1550F Film Polyethylene
(discontinued **) Polyethylene 1550F is a low density polyethylene that contains no additives.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no long.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D3985 |
Eastman 184MF Polyethylene Film
(discontinued **) Polyethylene 184MF is a low-density formulation with medium slip and low antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is character.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D3985 |
Eastman 1925F Polyethylene Film
(discontinued **) Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman 1810F Polyethylene
(discontinued **) Polyethylene 1810F is a fractional-melt low-density formulation with no slip or antiblock. It is suggested for film applications requiring high impact strength, high tear strength and very good opt.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman 1830F Polyethylene
(discontinued **) Polyethylene 1830F is a low-density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat sealing range and.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman 1840F Polyethylene
(discontinued **) Polyethylene 1840F is a low-density formulation with no slip or antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is characterized by.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman E6838-795F Polyethylene
(discontinued **) E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman E6838-796F Polyethylene
(discontinued **) E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman E6838-899F Polyethylene
(discontinued **) E6838-899F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat-sealing range, and good pr.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman E6838-922F Polyethylene
(discontinued **) E6838-922F is a low density formulation with medium slip and medium antiblock. Outstanding optical properties make this material an excellent choice for food packaging applications.List of Applicat.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman E6838-969F Polyethylene
(discontinued **) E6838-969F is a low density formulation with no slip and medium antiblock. It is suggested for film applications that require toughness such as shrink/bundling film, disposable diapersand overwrap... |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman E6838-997F Polyethylene
(discontinued **) E6838-997F natural is a low density formulation with no slip or antiblock. Outstanding optical properties make this material an excellent choice for calendering and as a clarity filler in co-extrud.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman D4036-F Polyethylene
(discontinued **) D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman D4052-F Polyethylene
(discontinued **) D4052-F is a fractional-melt low density formulation with low slip and low antiblock. It is suggested for film applications requiring impact strength, outstanding clarity, and good tear resistance... |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman E6838-963F Polyethylene
(discontinued **) E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |
|||
Oxygen Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman E6838-975F Polyethylene
(discontinued **) E6838-975F is a low density formulation with medium slip and medium antiblock. The formula is used in general purpose packaging where impact strength and processability are important. End-use film.. |