Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 1.70 cc-mm/m²-24hr-atm | 4.32 cc-mil/100 in²-24hr-atm | or 140 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® HS Polyester Film, 48 Gauge (12 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |
|||
Oxygen Transmission | 1.70 cc-mm/m²-24hr-atm | 4.32 cc-mil/100 in²-24hr-atm | or 140 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® LB Polyester Film, 48 Gauge (12 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film designed for use as a component of a lamination. Standard thickness offered include 48, 75, and 92 gauges. Variet.. |
|||
Oxygen Transmission | 1.70 cc-mm/m²-24hr-atm | 4.32 cc-mil/100 in²-24hr-atm | or 75 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® LB Polyester Film, 92 Gauge (23 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film designed for use as a component of a lamination. Standard thickness offered include 48, 75, and 92 gauges. Variet.. |
|||
Oxygen Transmission | 1.70 cc-mm/m²-24hr-atm | 4.32 cc-mil/100 in²-24hr-atm | or 140 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® LBT Polyester Film, 48 Gauge (12 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film that has been corona-treated to provide superior wetting and adhesion to inks, primers, and adhesives. Standard th.. |
|||
Oxygen Transmission | 1.70 cc-mm/m²-24hr-atm | 4.32 cc-mil/100 in²-24hr-atm | or 75 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® LBT Polyester Film, 92 Gauge (23 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film that has been corona-treated to provide superior wetting and adhesion to inks, primers, and adhesives. Standard th.. |
|||
Oxygen Transmission | 1.70 cc-mm/m²-24hr-atm | 4.32 cc-mil/100 in²-24hr-atm | Tested per ASTM D3985 at 22°C |
DuPont Teijin Films Mylar® LBT-2 Polyester Packaging Film, 48 Gauge Data provided by DuPont Packaging Polymers.Mylar® LBT-2 is an uncoated, transparent, exceptionally strong film used as a substrate for laminating and extrusion coating and as a component of packagi.. |