Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 0.110 cc-mm/m²-24hr-atm | 0.279 cc-mil/100 in²-24hr-atm | or 6 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® M45 Polyester Film, 75 Gauge (22 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, dispersion coated on one side with a PVDC copolymer. The coating is an excellent moisture and oxygen barrier. M45.. |