Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 0.0140 cc-mm/m²-24hr-atm | 0.0356 cc-mil/100 in²-24hr-atm | 20°C- 65% RH; based on 20 µm layer |
Noltex Soarnol® ET3803 Ethylene Vinyl Alcohol Copolymer Medium ethylene content. Suitable for packaging a wet product in a wet environment. Preferred for use in forming webs for meat and cheese packaging. Ethylene content 38 mol%. Volatile matter 0.3%... |
|||
Oxygen Transmission | 0.0140 cc-mm/m²-24hr-atm | 0.0356 cc-mil/100 in²-24hr-atm | 20°C- 65% RH; based on 20 µm layer |
Noltex Soarnol® ET3808 Ethylene Vinyl Alcohol Copolymer Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Oxygen Transmission | 0.0140 cc-mm/m²-24hr-atm | 0.0356 cc-mil/100 in²-24hr-atm | 20°C; 65% RH; Permeability increases significantly at higher moisture content. |
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th.. |
|||
Oxygen Transmission | 0.0140 cc-mm/m²-24hr-atm | 0.0356 cc-mil/100 in²-24hr-atm | 20°C; 65% RH; Permeability increases significantly at higher moisture content. |
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |
|||
Oxygen Transmission | 0.0140 cc-mm/m²-24hr-atm | 0.0356 cc-mil/100 in²-24hr-atm | |
Dow Saran® F-239 PVDC SARAN® barrier resin F-239 is used for coating cellophane and polyester film. It is applied from a tetrahydrofuran/toluene solvent system, and gives coatings with excellent adhesion and transparenc.. |