Physical Properties Metric English Comments
Oxygen Transmission 0.00400 - 0.600 cc-mm/m²-24hr-atm
0.0102 - 1.52 cc-mil/100 in²-24hr-atm
Average value: 0.0397 cc-mm/m²-24hr-atm Grade Count:28
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
Oxygen Transmission 0.00400 cc-mm/m²-24hr-atm
0.0102 cc-mil/100 in²-24hr-atm
20°C; 65% RH; Permeability increases significantly at higher moisture content.
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas ..
Oxygen Transmission 0.00400 cc-mm/m²-24hr-atm
0.0102 cc-mil/100 in²-24hr-atm
Dow Saran® 516 PVDC
SARAN® 516 barrier polymer, a copolymer of vinylidene chloride and vinyl chloride, designed for sheet coextrusion and forming into rigid plastic barrier containers for food applications. It is supp..
Oxygen Transmission 0.00400 cc-mm/m²-24hr-atm
0.0102 cc-mil/100 in²-24hr-atm
Dow Saran® 525 PVDC
SARAN® 525 barrier polymer, a copolymer of vinylidene chloride and vinyl chloride, designed for sheet coextrusion and forming into rigid plastic barrier containers for food applications. It is supp..
Oxygen Transmission 0.00400 cc-mm/m²-24hr-atm
0.0102 cc-mil/100 in²-24hr-atm
Dow Saran® 469 PVDC
SARAN® 469 barrier polymer with a molecular weight of 83000, is a copolymer of vinylidene chloride and vinyl chloride, designed for cast film extrusion and coextrusion into barrier films used in fl..
Oxygen Transmission 0.00400 - 0.0470 cc-mm/m²-24hr-atm
0.0102 - 0.119 cc-mil/100 in²-24hr-atm
Average value: 0.0219 cc-mm/m²-24hr-atm Grade Count:10
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..
Oxygen Transmission 0.00400 cc-mm/m²-24hr-atm
0.0102 cc-mil/100 in²-24hr-atm
20°C; 65% RH; Permeability increases significantly at higher moisture content.
EVALCA EVAL® EF-XL Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
Biaxially oriented type film; property values for 15 µm film.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produ..