Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 99 g/10 min @Load 10.0 kg, Temperature 220 °C |
99 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 (G) |
LG Chemical HIPS MI730 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |