Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 96 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 96 g/10 min

@Load 5.00 kg,
Temperature 230 °C
96 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Borealis Xmod™ BG055AI High Stiffness Polypropylene for Injection Molding Applications
Xmod BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. Xmod BG055AI is a very easy flowing material with a good balance between impact strength..
Copyright © lookpolymers.com All Rights Reserved