Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 9.5 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 9.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
9.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) BL 4M HM 8355 High Density Polyethylene
BL4M is a high density polyethylene with 1-Butene as co monomer. It is high molar mass, easily processable, high stiffness and strength, good SCR, very good molding surface finish.Applications: jer..
Melt Flow 9.5 g/10 min

@Load 1.20 kg,
Temperature 250 °C
9.5 g/10 min

@Load 2.65 lb,
Temperature 482 °F
ASTM D 1238
SABIC Innovative Plastics PC6300 PC
PC6300 resin is a very high flow (MFR = 9.5 at 250ºC/1.2kg) polycarbonate product designed for use in the optical media market.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 9.5 g/10 min

@Load 1.20 kg,
Temperature 250 °C
9.5 g/10 min

@Load 2.65 lb,
Temperature 482 °F
ASTM D 1238
SABIC Innovative Plastics PC6300 PC (Asia Pacific)
PC6300 resin is a very high flow (MFR = 9.5 at 250ºC/1.2kg) polycarbonate product designed for use in the optical media market.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 9.5 g/10 min

@Load 1.20 kg,
Temperature 250 °C
9.5 g/10 min

@Load 2.65 lb,
Temperature 482 °F
ASTM D 1238
SABIC Innovative Plastics PC6300 PC (Europe-Africa-Middle East)
PC6300 resin is a very high flow (MFR = 9.5 at 250ºC/1.2kg) polycarbonate product designed for use in the optical media market.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
Melt Flow 9.5 g/10 min

@Load 6.60 kg,
Temperature 337 °C
9.5 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem 2412EPR PEI
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am..
Melt Flow 9.5 g/10 min

@Load 6.60 kg,
Temperature 337 °C
9.5 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As..
Melt Flow 9.5 g/10 min

@Load 6.60 kg,
Temperature 337 °C
9.5 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
Melt Flow 9.5 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.5 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ISO 1133
Styron Pulse® A20-95 PC/ABS
A medium impact strength PC/ABS blend with high heat distortion and excellent processability.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Melt Flow 9.5 g/10 min

@Load 5.00 kg,
Temperature 230 °C
9.5 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Borealis Borclean™ HB311BF Polypropylene Homopolymer for Capacitor Film
Borclean HB311BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HB311BF does not contain slip, antiblock, antist..
Melt Flow 9.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
9.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Diamond Polymers SAN 263 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 9.5 g/10 min

@Load 10.0 kg,
Temperature 230 °C
9.5 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ISO 1133
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved