Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
9.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 1501 Description: Injection Molding GradeInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 9.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
9.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 1502 Description: Injection Molding Grade, High GlossInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 9.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
9.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS VP-12 Description: Flame Retardant with UVInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 9.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
9.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS VP-11 Description: Flame Retardant ABSInformation provided by Diamond Polymers, Inc. |