Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 81 g/10 min @Load 5.00 kg, Temperature 260 °C |
81 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications. |
|||
Melt Flow | 81 g/10 min @Load 5.00 kg, Temperature 260 °C |
81 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications. |
|||
Melt Flow | 81 g/10 min @Load 10.0 kg, Temperature 220 °C |
81 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 (G) |
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |