Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 8.8 g/10 min

@Load 10.0 kg,
Temperature 220 °C
8.8 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
SABIC Innovative Plastics Geloy XTWM206 ASA
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 8.8 g/10 min

@Load 10.0 kg,
Temperature 220 °C
8.8 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
SABIC Innovative Plastics Geloy XTWM206 ASA (Asia Pacific)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Asia Pacific regio..
Melt Flow 8.8 g/10 min

@Load 10.0 kg,
Temperature 220 °C
8.8 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Melt Flow 8.8 g/10 min

@Load 3.80 kg,
Temperature 230 °C
8.8 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Cond I; ASTM D1238
Ravago Manufacturing Americas Hylac® GP74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Melt Flow 8.8 g/10 min

@Load 6.60 kg,
Temperature 337 °C
8.8 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem 1100FV PEI
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
Melt Flow 8.8 g/10 min

@Load 6.60 kg,
Temperature 337 °C
8.8 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
Melt Flow 8.8 g/10 min

@Load 6.60 kg,
Temperature 337 °C
8.8 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
Melt Flow 8.8 g/10 min

@Load 6.60 kg,
Temperature 337 °C
8.8 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem 1100V PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle Eas..