Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.3 g/10 min @Load 1.00 kg, Temperature 235 °C |
8.3 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 0615 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 8.3 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.3 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 8.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Topas Advanced Polymers TOPAS® 5013F-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013F-04 is a high temperature film extrusion grade for blends. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity .. |
|||
Melt Flow | 8.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 3500 Natural 1050 Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 8.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 4500R Description: Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 8.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ABS 4501 Injection Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 8.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 4502 Description: Injection Molding Grade, Medium Impact Information provided by Diamond Polymers, Inc. |
|||
Melt Flow | 8.3 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.3 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed.. |