Physical Properties Metric English Comments
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Eraclene® MP 90 C High Density Polyethylene - Injection Molding
Eraclene MP 90 C is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution and a high ..
Melt Flow 7.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
7.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
SABIC FI0750 Bimodal High Density Polyethylene for Blown Film
Product Description: FI0750 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Melt Flow 7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Network Polymers SAN 277 Blue Tint Color
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
Melt Flow 7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Network Polymers SAN 278 Medium Blue Tint
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
Melt Flow 7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Network Polymers SAN 279 Water White Color
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
Melt Flow 7.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East)
Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im..
Melt Flow 7.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
7.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) BL8 HM 7745 High Density Polyethylene
BL8 (HM 7745) is a high density polyethylene with Butene-1 as comonomer.Applications: for heating oil storage tanks, large containers for various chemicals.Information provided by Iran Petrochemical..
Melt Flow 7.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
7.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene
EX 4HS is a high density polyethylene with 1-Butene as co monomer. It has high rigidity, low gel level, high drawdown, very high stiffness and good tenacity.Applications: film extrusion, blending ..
Melt Flow 7.5 g/10 min

@Load 5.00 kg,
Temperature 280 °C
7.5 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D 1238
SABIC Innovative Plastics Noryl MX5569 PPE+PS
PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-..
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 220 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 428 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Melt Flow 7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 3001MC
Description: Plating GradeInformation provided by Diamond Polymers, Inc.
Melt Flow 7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 3002MC
Description: Plating GradeInformation provided by Diamond Polymers, Inc.
Melt Flow 7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 3300
Description: General Purpose Utility BlackInformation provided by Diamond Polymers, Inc.
Melt Flow 7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 3501
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 3501 Natural 1050
Description: Natural, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 3502
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS/PC FC-30
Description: Injection Molding Grade, High Impact, Flame RetardantInformation provided by Diamond Polymers, Inc.
Melt Flow 7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238