Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
6.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® MG37EPX ABS ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L) |