Physical Properties Metric English Comments
Melt Flow 6.5 - 16 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.5 - 16 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Kazanorgsintez PE80B-275 Medium Density Polyethylene Composite
Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc..
Melt Flow 6.5 - 16 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.5 - 16 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Kazanorgsintez PE80B-286 Medium Density Polyethylene Composite
Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc..
Melt Flow 6.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM-D1238
Ineos ABS Lustran® 720 ABS, Molding Grade
Lustran® ABS 720 resin is a black, virgin injection molding grade of ABS (acrylonitrile butadiene styrene). It is supplied as salt-and-pepper pellets with color concentrate 901802 black. Designed..
Melt Flow 6.5 g/10 min

@Load 2.16 kg,
Temperature 250 °C
6.5 g/10 min

@Load 4.76 lb,
Temperature 482 °F
Part; ISO 1133
DuPont Performance Polymers Crastin® CE2056 NC010 PBT
Crastin® CE2056 NC010 is an unreinforced polybutylene terephthalate molding resin.Information provided by DuPont Performance Polymers
Melt Flow 6.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Chi Mei Kibisan® PN-127 SAN
Heat Resistant
Melt Flow 6.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Chi Mei Kibisan® PN-127H SAN
Chemical Resistant
Melt Flow 6.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
6.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® EXL1033C PC Copolymer
Lexan*EXL1033C polycarbonate (PC) siloxane copolymer resin is a low flow, UV stabilized grade designed for (co)-extrusion. This resin offers low temperature (-30C) ductility and excellent extrusion ..