Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 6.4 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 6.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D 1238
SABIC Innovative Plastics Cycolac® INP562 ABS
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Melt Flow 6.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Melt Flow 6.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
EVALCA EVAL® G156A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
48 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, specialty applications. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now p..
Melt Flow 6.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238, ISO 1133
DuPont™ Appeel® 22D843 Ethylene Acrylate
DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable ..
Melt Flow 6.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Diamond Polymers ABS 7401 Injection Molding Grade, Extra High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 6.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 7502
Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 6.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 7501
Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.