Physical Properties Metric English Comments
Melt Flow 6.2 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.2 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
SABIC P6006 Black High Density Polyethylene for Pipes
Product Description: P6006 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio..
Melt Flow 6.2 g/10 min

@Load 2.16 kg,
Temperature 260 °C
6.2 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Ravago Manufacturing Americas Hybrid S466 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Melt Flow 6.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
LG Chemical 81HF SAN Resin
High flow, Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include food receptacles, disposable li..
Melt Flow 6.2 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.2 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) EX 3 – 100S HM CRP 100 N High Density Polyethylene
EX3-100S is a high density polyethylene with 1-Butene as co monomer. It is natural, outstanding ESCR, high impact strength, outstanding hydrostatic strength for PE 100 class.Applications: pipe extr..
Melt Flow 6.2 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.2 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 3003MC Black 1722
Description: BlackInformation provided by Diamond Polymers, Inc.
Melt Flow 6.2 g/10 min

@Load 3.80 kg,
Temperature 300 °C
6.2 g/10 min

@Load 8.38 lb,
Temperature 572 °F
ASTM D1238
Diamond Polymers DIAMALOY 627 PC/Polyester Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 6.2 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.2 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Styrolution NAS® 21 Acrylic Copolymer
Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma..