Physical Properties Metric English Comments
Melt Flow 57 g/10 min

@Load 5.00 kg,
Temperature 200 °C
57 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Versaflex™ 9570-1 Thermoplastic Elastomer (TPE)
Versaflex™ 9570-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Melt Flow 57 g/10 min

@Load 5.00 kg,
Temperature 200 °C
57 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Versaflex™ 9570-9 Thermoplastic Elastomer (TPE)
Versaflex™ 9570-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Melt Flow 57 g/10 min

@Load 5.00 kg,
Temperature 300 °C
57 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics LNP THERMOCOMP D451 PC (Asia Pacific)
LNP* Thermocomp* D451 (or EXTC8141) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good duc..
Melt Flow 57 g/10 min

@Load 5.00 kg,
Temperature 230 °C
57 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer
Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 h..