Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycolac® INP572 ABS High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Melt Flow | 5.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® INP572 ABS+SAN High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Melt Flow | 5.8 g/10 min @Load 10.0 kg, Temperature 190 °C |
5.8 g/10 min @Load 22.0 lb, Temperature 374 °F |
ExxonMobil Method |
ExxonMobil Pax-Plus™ 3204 Blown Film Resin Pax-Plus 3204 is a rubber modified high density polyethylene film resin which is used primarily in film requiring good impact strength. It is specially formulated to provide easy tear in the machin.. |