Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.7 g/10 min @Load 2.16 kg, Temperature 260 °C |
5.7 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |