Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 47 g/10 min @Load 10.0 kg, Temperature 220 °C |
47 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® INP563 ABS SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Melt Flow | 47 g/10 min @Load 10.0 kg, Temperature 220 °C |
47 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® INP563 ABS+SAN SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Melt Flow | 47 g/10 min @Load 10.0 kg, Temperature 250 °C |
47 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 47 g/10 min @Load 10.0 kg, Temperature 250 °C |
47 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 47 g/10 min @Load 10.0 kg, Temperature 220 °C |
47 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Denka TH-21 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |