Polymer Property : Melt Flow = 46 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 46 g/10 min

@Load 21.6 kg,
Temperature 190 °C
46 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
SABIC B4660/B4660AB High Density Polyethylene for Blow Molding
Product Description: B4660 series grades are medium molecular weight High Density Polyethylene homopolymer for blow molding applications. They are primarily designed for imparting high rigidity, t..
Melt Flow 46 g/10 min

@Load 21.6 kg,
Temperature 190 °C
46 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
SABIC F04660 High Density Polyethylene for Blown Film Applications
Product Description: F04660 is a homopolymer HDPE film grade with excellent processability and high stiffness. It has good moisture barrier properties and can be blended with LDPE and LLDPE to imp..
Melt Flow 46 g/10 min

@Load 21.6 kg,
Temperature 190 °C
46 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
SABIC BM6246LS High Density Polyethylene for Blow Molding
Product Description: BM6246LS grade is a medium molecular weight High Density Polyethylene homopolymer for blow molding applications. It is primarily designed for imparting high rigidity, toughnes..
Melt Flow 46 g/10 min

@Load 10.0 kg,
Temperature 220 °C
46 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238(G)
LG Chemical ALPHALAC SG910 HIPS
High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA..
Melt Flow 46 g/10 min

@Load 5.00 kg,
Temperature 260 °C
46 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..
Melt Flow 46 g/10 min

@Load 21.6 kg,
Temperature 190 °C
46 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil HDPE HYA 800 High Density Polyethylene Resin
Product Description: HYA 800 is a homopolymer HDPE grade, characterized by high stiffness, high rigidity and high flow.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal ..