Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 45 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 45 - 65 g/10 min

@Load 5.00 kg,
Temperature 200 °C
45 - 65 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE)
The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 260 °C
45 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 260 °C
45 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific)
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 260 °C
45 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
Melt Flow 45 g/10 min

@Load 1.20 kg,
Temperature 300 °C
45 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® ML7677A PC (Asia Pacific)
Commercial grade for Polycarbonate in only nature color. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm.This data was supplied by SABIC-IP for the Asia Pacific reg..
Melt Flow 45 g/10 min

@Load 1.20 kg,
Temperature 300 °C
45 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm.
Melt Flow 45 g/10 min

@Load 1.20 kg,
Temperature 300 °C
45 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm.
Melt Flow 45 g/10 min

@Load 1.20 kg,
Temperature 300 °C
45 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East)
Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm.
Melt Flow 45 g/10 min

@Load 21.6 kg,
Temperature 190 °C
45 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Eraclene® PF 92 High Density Polyethylene - Pipe Grade Resin
Eraclene PF 92 is a homopolymer high density polyethylene resin (HDPE) with antioxidants, suitable for pipe application. It is characterized by high rigidity, high impact strength and low swelling...
Melt Flow 45 g/10 min

@Load 1.20 kg,
Temperature 300 °C
45 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific)
Transparent Polycarbonate in natural color. Excellent processability, super high flow.
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 265 °C
45 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 266 °C
45 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 265 °C
45 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East)
VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 280 °C
45 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D 1238
SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific)
High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 220 °C
45 g/10 min

@Load 4.76 lb,
Temperature 428 °F
ASTM D1238
Lubrizol Estane® UB310 Thermoplastic Polyurethane
Type: Estane® UB310 is a Shore 95A, polyester based, hot melt adhesive with excellent low temperature flexibility thermoplastic polyurethane (TPU).Uses: Extrusion, Powder Coating, Ideal for Fire Ho..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 230 °C
45 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled
Daplen EE137AI is a 10% mineral filled grade intended for injection molding. EE137AI has been developed especially for the car industry, to be used in interior parts where high scratch resistance i..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 230 °C
45 g/10 min

@Load 11.0 lb,
Temperature 446 °F
Volume Resistivity 1000 ohm-cm
TIMCAL ENSACO™ 250G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
Melt Flow 45 g/10 min

@Load 10.0 kg,
Temperature 220 °C
45 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO-1133
Chi Mei Polylac® PA-756 ABS - High Flow
High rigid, high flow
Melt Flow >= 45 g/10 min

@Load 10.0 kg,
Temperature 400 °C
>= 45 g/10 min

@Load 22.0 lb,
Temperature 752 °F
BASF Ultrason® E 2010 C6 30% Carbon Filled
Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu..
Copyright © lookpolymers.com All Rights Reserved