Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 40 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 40 g/10 min

@Load 10.0 kg,
Temperature 220 °C
40 g/10 min

@Load 22.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycolac® MG34LGHF ABS
Low gloss, high flow ABS for unpainted interior applications.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 330 °C
40 g/10 min

@Load 4.76 lb,
Temperature 626 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Asia Pacific)
Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 330 °C
40 g/10 min

@Load 4.76 lb,
Temperature 626 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Europe-Africa-Middle East)
Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 330 °C
40 g/10 min

@Load 4.76 lb,
Temperature 626 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® 4301 PPC+PC
Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Americas region.
Melt Flow 40 g/10 min

@Load 10.0 kg,
Temperature 220 °C
40 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Kingfa FW-620 Flame Retardant ABS
Features:UL 94 V-0 @ 1.5-3.0mmWeather resistanceHeat resistanceGood surfaceApplications:Injection moldingOA deviceChargerTransformerInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Flow 40 g/10 min

@Load 10.0 kg,
Temperature 220 °C
40 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Kingfa HF-618 Flame Retardant ABS
Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Flow 40 g/10 min

@Load 10.0 kg,
Temperature 220 °C
40 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Kingfa HP-126 Modified ABS
Features:UL94 HB @ 1.6-3.0mmHigh impact resistanceHigh flowApplications:LCD cabinetLarge thin-wall partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 340 °C
40 g/10 min

@Load 11.0 lb,
Temperature 644 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 340 °C
40 g/10 min

@Load 11.0 lb,
Temperature 644 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 340 °C
40 g/10 min

@Load 11.0 lb,
Temperature 644 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Europe-Africa-Middle East)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 40 g/10 min

@Load 10.0 kg,
Temperature 345 °C
40 g/10 min

@Load 22.0 lb,
Temperature 653 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East)
High flow Ultem for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 266 °C
40 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East)
VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles.
Melt Flow 40 g/10 min

@Load 6.60 kg,
Temperature 337 °C
40 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem ATX102R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 40 g/10 min

@Load 6.60 kg,
Temperature 337 °C
40 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 40 g/10 min

@Load 6.60 kg,
Temperature 337 °C
40 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region..
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 360 °C
40 g/10 min

@Load 11.0 lb,
Temperature 680 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr..
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 265 °C
40 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East)
10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 250 °C
40 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ISO 1133
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East)
Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas..
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 230 °C
40 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Borealis Daplen™ EE188AI Polypropylene TPO Compound
Daplen™ EE188AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. ..
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 230 °C
40 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Borealis Daplen™ EE189AI Polypropylene TPO Compound
Daplen™ EE189AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. ..
Melt Flow 40 g/10 min

@Load 21.6 kg,
Temperature 190 °C
40 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM-D1238
Braskem GD5160 HDPE Blow Molding Polyethylene Homopolymer
GD5160 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance and productivity. It was developed for the blow-molding segment. It is used in ..
Melt Flow 40 g/10 min

@Load 1.20 kg,
Temperature 300 °C
40 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer
40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 230 °C
40 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
PolyOne Elastamax XL 0233-1 Polyurethane Compound  (discontinued **)
This is a static dissipative thermoplastic polyurethane compound for injection molding and extrusion applications. Physical Form: Pellet. Standard Color: Black/grey.Information provided by M. A. H..
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 360 °C
40 g/10 min

@Load 11.0 lb,
Temperature 680 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem ATX103R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r..
Melt Flow 40 g/10 min

@Load 5.00 kg,
Temperature 360 °C
40 g/10 min

@Load 11.0 lb,
Temperature 680 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif..