Polymer Property : Melt Flow = 4.5 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Eraclene® MM 74 U High Density Polyethylene - Injection Molding
Eraclene MM 74 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution. The polym..
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 275 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound
PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1..
Melt Flow 4.5 - 7.2 g/10 min

@Load 21.6 kg,
Temperature 190 °C
4.5 - 7.2 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 4.5 - 7.2 g/10 min

@Load 21.6 kg,
Temperature 190 °C
4.5 - 7.2 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 6948C (486H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Ravago Manufacturing Americas Hylac® HF143 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Eraclene® MM 74 High Density Polyethylene - Injection Molding
Eraclene MM 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 74 is characterized by a good balance between rigidity and impact..
Melt Flow 4.5 - 7.2 g/10 min

@Load 21.6 kg,
Temperature 190 °C
4.5 - 7.2 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 6949C (486H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Kingfa HF-626 Flame Retardant ABS
Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowHigh impact resistanceApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Flow 4.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM-D1238
Ineos ABS Lustran® 633 ABS, Injection Molding Grade
Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical ..
Melt Flow 4.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Techmer ES Plastiblend® ABS NAT
Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: Natural ColorInformation provided by TP Composites, Inc.
Melt Flow 4.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Styron EMERGEâ„¢ 7100 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Overview: EMERGEâ„¢ PC/ABS 7100 advanced resin exhibits a balance of properties between impact strength, heat resistance and processability. Its superior natural base color and lot-to-lot color ..
Melt Flow 4.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Techmer ES Plastiblend® ABS LE BK
Availability: North AmericaForms: PelletsFeatures: Low ExtractablesAppearance: BlackInformation provided by TP Composites, Inc.
Melt Flow 4.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin
Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can ..
Melt Flow 4.5 g/10 min

@Load 3.80 kg,
Temperature 260 °C
4.5 g/10 min

@Load 8.38 lb,
Temperature 500 °F
ISO 1133
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin
Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can ..
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Borealis HC101BF Polypropylene Homopolymer
HC101BF is a polypropylene homopolymer. Applications: HC101BF has been developed especially for applications like: co-extrusion applications, print lamination, metallisable film, coated film, packa..
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
ExxonMobil Exact™ 9371 Ethylene-based Plastomer Resin
Product Description: Exact 9371 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P..
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Exact™ 9371 Ethylene-based Plastomer Resin
Product Description: Exact 9371 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P..
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Chi Mei Kibiton® PB-575 SBC
Shoe sole industrial accessory
Melt Flow 4.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
4.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO-1133
Chi Mei Polylac® PA-709S ABS - Extrusion
Super Impact Extrusion
Melt Flow 4.5 g/10 min

@Load 10.0 kg,
Temperature 250 °C
4.5 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ISO 1133
DuPont Performance Polymers Hytrel® BM6574 BK316 TPC-ET  (Unverified Data**)
Hytrel® BM6574 is a 65 nom. Shore D, plasticiser free high performance resin for blow molding and extrusion; it shows ageing resistance up to 150°C, and excellent mechanical properties at elevated..
Melt Flow 4.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 9502
Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc.