Polymer Property : Melt Flow = 4.2 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 4.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
I. Stern 750SW Medium Impact Natural ABS
Features:Easy color-abilityInjection MoldingApplicationsOffice equipmentElectronic partsSpools, ReelsInformation provided by I. Stern & Co. Inc.
Melt Flow 4.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
SABIC Innovative Plastics Noryl PX5622 PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. Good flow and surface aesthetics. UL94 V0/5VA/5VB. RTI Elec/Imp/Str 65. Suitable for E/E market indoor/outdoor applications.This da..
Melt Flow 4.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Supreme Petrochem SP 6503 High Impact Polystyrene
Characteristics High Impact Available in various colors Easy flow High stiffness Processing Injection moldingApplications Computer cabinet, printer body, business machine housing etc. Material St..
Melt Flow 4.2 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.2 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 3003 MC
Description: High Heat Plating GradeInformation provided by Diamond Polymers, Inc.
Melt Flow 4.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Chi Mei Polylac® PA-765B ABS - Flame Retardant
F.R. Medium Impact