Physical Properties Metric English Comments
Melt Flow 38 g/10 min

@Load 5.00 kg,
Temperature 200 °C
38 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE)
Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora..
Melt Flow 38 g/10 min

@Load 5.00 kg,
Temperature 200 °C
38 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell..
Melt Flow 38 g/10 min

@Load 5.00 kg,
Temperature 200 °C
38 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell..
Melt Flow 38 g/10 min

@Load 5.00 kg,
Temperature 260 °C
38 g/10 min

@Load 11.0 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East)
High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 38 g/10 min

@Load 21.6 kg,
Temperature 220 °C
38 g/10 min

@Load 47.6 lb,
Temperature 428 °F
ASTM D 1238
Cossa Polimeri ESTALUX 9206 A Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l.
Melt Flow 38 g/10 min

@Load 21.6 kg,
Temperature 220 °C
38 g/10 min

@Load 47.6 lb,
Temperature 428 °F
ASTM D 1238
Cossa Polimeri ESTALUX 9206 Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information..
Melt Flow 38 g/10 min

@Load 10.0 kg,
Temperature 220 °C
38 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO-1133
Chi Mei Polylac® PA-716 ABS - High Flow
High flow, medium impact
Melt Flow 38 g/10 min

@Load 1.20 kg,
Temperature 300 °C
38 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer
40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.